Painting

Builders,

He is a quick tip on painting your ring gear. I put it on a plastic cup, and paint it horizontally. It resists runs a lot better. I then flip it over and do the other side.

.

After it dries, I hang in on a wire in my shop oven and bake it for 20 minutes at 300F. I do this last step in Florida because the very high humidity tends to blush very fast drying paint. The time in the oven makes it glossy again.

.

.

This is the only brand of paint I use on engines. It is vastly better than other paints I have tried .

.

.

Ready to bake.

.

William